Industrial Laminates/Norplex NP180 Synthetic Fabric
Subcategory: Aramid; Thermoset
Key Words: Micarta
Material Notes: Description: aramid fabric material with a high performance epoxy resin matrix. Excellent electrical and mechanical properties at elevated temperatures and in adverse environments. Thickness Tested: 0.062", 0.125", and 0.500" Information provided by Industrial Laminates/Norplex.
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Hardness, Rockwell M
- Tensile Strength, Yield
- Flexural Strength
- Compressive Strength
- Izod Impact, Unnotched
- Dielectric Constant
- Dielectric Strength
- Dielectric Breakdown
- Dissipation Factor
- Arc Resistance
- CTE, linear 20°C
- CTE, linear 100°C
- Maximum Service Temperature, Air
- Glass Temperature
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|