Industrial Laminates/Norplex NP193P Synthetic Fabric
Subcategory: Aramid; Phenolic; Thermoset
Key Words: Micarta
Material Notes: Description: 17 oz. aramid and "soft glass" fibers are combined to make a fabric that is stronger than pure aramid and less abrasive than glass fabrics. This material is impregnated with a high temperature phenolic resin matrix, which produces a composite with excellent mechanical strength at elevated temperatures and adverse environments. Applications include wear plates for conveyor systems, valve plates, and compressor and pump vanes. Variations of this material may be developed for specific applications. Thickness Tested: 0.125", 0.250" & 0.500" Information provided by Industrial Laminates/Norplex.
| Available Properties |
- Moisture Absorption at Equilibrium
- Tensile Strength, Yield
- Modulus of Elasticity
- Flexural Strength
- Compressive Strength
- Izod Impact, Unnotched
- Dielectric Constant
- Dissipation Factor
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Flammability, UL94
- Bond Strength
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|