Industrial Laminates/Norplex NP555 Carbon Fiber
Subcategory: Phenolic; Thermoset; Carbon Fiber/Thermoset Composite
Key Words: Micarta
Material Notes: Description: NP555 is composed of carbon fiber fabric and a phenolic resin system. It has excellent moisture resistance and physical properties. This material was designed to replace asbestos vane material for large, high performance compressors. Thickness Tested: 0.062", 0.125" and 0.500" Information provided by Industrial Laminates/Norplex.
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Hardness, Rockwell M
- Tensile Strength, Yield
- Modulus of Elasticity
- Flexural Strength
- Izod Impact, Unnotched
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Maximum Service Temperature, Air
- Flammability, UL94
- Bond Strength
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|