Industrial Laminates/Norplex NP185 Carbon Fiber
Subcategory: Aramid; Phenolic; Thermoset; Carbon Fiber/Thermoset Composite
Key Words: Micarta
Material Notes: Description: NP185, aramid fiber fabric/phenolic surfaces (2 ply each side) on NP504 core material. Excellent mechanical properties at elevated temperatures and in adverse environments. Used as wear strips in high temperature environments. Thickness Tested: 0.250" Information provided by Industrial Laminates/Norplex.
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Flexural Strength
- Izod Impact, Unnotched
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |