Industrial Laminates/Norplex NP310AG Cotton Fabric Base Laminate
Subcategory: Phenolic; Thermoset
Key Words: Micarta
Material Notes: Description: Cotton phenolic laminate similar to NEMA Grade C, with non-afterglow properties similar to Grade CF, NEMA LI-1-1998. Information provided by Industrial Laminates/Norplex.
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Hardness, Rockwell M
- Flexural Strength
- Izod Impact, Unnotched
- Dielectric Breakdown
- Bond Strength
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|