Industrial Laminates/Norplex NP501 Glass Fabric Base Laminate
Subcategory: Glass; Glass Fiber; Thermoset
Key Words: Micarta
Material Notes: Description: Woven glass fabric with epoxy resin system. Engineered to provide improved properties over NEMA Grade FR-4 in applications involving thermal stress, such as reflow and solder pallets. Information provided by Industrial Laminates/Norplex.
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Hardness, Rockwell M
- Tensile Strength, Yield
- Modulus of Elasticity
- Flexural Strength
- Compressive Strength
- Shear Strength
- Izod Impact, Unnotched
- Dielectric Constant
- Dielectric Breakdown
- Dissipation Factor
- Arc Resistance
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Maximum Service Temperature, Air
- Glass Temperature
- Flammability, UL94
- Bond Strength
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|