Ineos 3950 Polypropylene Impact Copolymer
Subcategory: Polypropylene; Thermoplastic; Polymer
Key Words: Low gloss, high impact
Material Notes: Grade 3950 typically has a 35 melt flow rate and is a low gloss, high impact polypropylene copolymer. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520. Applications Benefits- Low gloss
- High impact resistance
| Available Properties |
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched, Low Temp
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Flammability Test
- Process
|
|
|
|
| Property Data |