Ineos L24G-00 Polypropylene Impact Copolymer
Subcategory: Polypropylene; Thermoplastic; Polymer
Key Words: Excellent impact resistance and a high flexural modulus
Material Notes: Grade L24G-00 is a high melt flow rate, antistatic high impact copolymer polypropylene for injection molding applications. It offers excellent impact resistance and a high flexural modulus. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520. Applications - Consumer products
- Housewares
- Automotive
Benefits- High impact resistance
- High flexural modulus
| Available Properties |
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched, Low Temp
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|