Ineos N20G-00 Polypropylene Impact Copolymer
Subcategory: Polypropylene; Thermoplastic; Polymer
Key Words: Very high impact resistance and good stiffness
Material Notes: Grade N20G-00 is a high melt flow rate “super-high” impact copolymer polypropylene for injection molding applications. It offers very high impact resistance and good stiffness. This material meets the requirements of the U.S Food and Drug Administration as specified in 21 CFR 177.1520. Applications - Toys
- Consumer products
- Housewares
- Automotive
- Compounding
Benefits- High melt flow rate
- Good stiffness
- Very high impact resistance
| Available Properties |
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched, Low Temp
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|