Ineos R01C-00 Polypropylene Random Copolymer
Subcategory: Polypropylene; Thermoplastic; Polymer
Key Words: High clarity random copolymer
Material Notes: Grade R01C-00 is a low flow rate, high clarity random copolymer designed for extrusion, thermoforming and blow molding, through it is clarifier/antistat additive combination. Applications that require good see-through clarity combined with good heat resistance and refrigerator temperature impact properties can benefit from the use of grade R01C-00. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520. Applications - Thermoformed packaging (cups, containers, lidding)
- Extrusion blow molded containers and bottles
- Injection blow molded containers and bottles
- Extruded sheet and profiles
Benefits- Excellent clarity
- Excellent processability
- Good impact resistance at room and refrigerator temperatures
- Low static charge
| Available Properties |
- Melt Flow
- Tensile Strength, Yield
- Flexural Modulus
- Izod Impact, Notched, Low Temp
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Haze
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|