Intercontinental Polymers PET Polymer Type 169-02 - Cationic, Semi-Dull, Polyester Pellets
Subcategory: Polyester, TP; Polyethylene Terephthalate (PET); Thermoplastic
Material Notes: Applications: Fiber Specialties Information provided by Intercontinental Polymers.
| Available Properties |
- Viscosity Measurement
- Gardner Color Number
- Melt Temperature
- Moisture Content
- COOH
- DEG
- TiO2
|
|
|
|
| Property Data |