Intercontinental Polymers HoPBT Polymer Type 545 - Clear, Polyester Pellets
Subcategory: Polyester, TP; Polybutylene Terephthalate (PBT); Thermoplastic
Material Notes: Applications: Engineering Resin Information provided by Intercontinental Polymers.
| Available Properties |
- Viscosity Measurement
- Melt Flow
- Gardner Color Number
- Melt Temperature
- Moisture Content
- Black Specks
- COOH
|
|
|
|
| Property Data |