IMI 73517 Solventless Polyester Varnish for Electrical Insulation
Subcategory: Polyester, TS; Thermoset
Key Words: Von Roll Isola USA; Insulating Materials Incorporated
Material Notes: Data provided by Von Roll Isola USA. IMI solventless resins provide relatively void-free insulation for greater protection agaist severe environments and corona breakdown. Flash Point: 30°C. Usage Notes: Bonding of high-speed armatures, auto generators, power tools, stators, transformers, coils, and capacitor impregnation. High heat distrortion laminating resin.
| Available Properties |
- Density
- Viscosity
- Dielectric Strength
- Maximum Service Temperature, Air
- Processing Temperature
|
|
|
|
| Property Data |