IMI 74001 Epoxy Varnish for Electrical Insulation
Subcategory: Epoxy; Thermoset
Key Words: Von Roll Isola USA; Insulating Materials Incorporated
Material Notes: Data provided by Von Roll Isola USA. Flash Point: 24°C. Average solids: 92.5%. Usage Notes: Clear epoxy insulating varnish which penetrates and saturates extremely well, giving outstanding moisture resistance and bond strength.
| Available Properties |
- Density
- Viscosity
- Dielectric Strength
- Maximum Service Temperature, Air
- Processing Temperature
|
|
|
|