Devcon Plastic Steel® Putty (A) Epoxy
Subcategory: Epoxy; Thermoset
Material Notes: General Repair Epoxy Comments: The original metal-filled epoxy putty used for hundreds of routine maintenance, production and tooling applications. Bonds to most metal, concrete and some plastics. Cures at room temperature and forms a tough, durable metallic mass. Can be drilled, tapped, machined or painted. Excellent resistance to oil, gasoline, water and many chemicals. Patch and repair areas where welding or brazing would be undesirable or impossible. Data provided by Ellsworth Adhesives.
| Available Properties |
- Density
- Hardness, Shore D
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Flexural Yield Strength
- Compressive Yield Strength
- Shear Strength
- Dielectric Constant
- Dielectric Strength
- CTE, linear 20°C
- Thermal Conductivity
- Maximum Service Temperature, Air
- Shrinkage
- Processing Temperature
- Pot Life
- Coverage per lb.
- Mix Ratio by Volume
- Mix Ratio by Weight
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|