Devcon Fastmeal™ Epoxy
Subcategory: Epoxy; Thermoset
Material Notes: Precision Repair Epoxy Comments: High-performance, alumina-filled epoxy putty for making fast, dependable emergency repair to leaks in pipes carrying ores, coal, cement, san and gravel. Cures in 5 minutes. Applies in temperatures as low as 40°F. Economical and convenient. Data provided by Ellsworth Adhesives.
| Available Properties |
- Density
- Hardness, Shore D
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Flexural Yield Strength
- Compressive Yield Strength
- Shear Strength
- Dielectric Constant
- Dielectric Strength
- CTE, linear 20°C
- Thermal Conductivity
- Maximum Service Temperature, Air
- Shrinkage
- Processing Temperature
- Pot Life
- Coverage per lb.
- Mix Ratio by Volume
- Mix Ratio by Weight
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|