Devcon Zip Patch™ Epoxy
Subcategory: Epoxy; Thermoset
Material Notes: Emergency Repair Products Comments: High-technology, adhesive-impregnated, putty patching system that cures at room temperature. Hardens to a tough, durable, waterproof finish in minutes. Easy-to-use, fast setting patch kit. Make permanent, waterproof field repairs to pipes, tanks and containers, Excellent adhesion to iron, steel, stainless steel, titanium, fiberglass, aluminum, wood, ceramics, composites, acrylics, PVC and most other plastics. Minimal surface preparation. Data provided by Ellsworth Adhesives.
| Available Properties |
- Density
- Viscosity
- Hardness, Shore D
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Flexural Yield Strength
- Shear Strength
- Dielectric Constant
- Dielectric Strength
- CTE, linear 20°C
- Thermal Conductivity
- Maximum Service Temperature, Air
- Shrinkage
- Processing Temperature
- Pot Life
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|