Juner® Halogen-Free Flame-Resistant Polyamide PA-A6 GF20%
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Material Notes: Applications: Shell of Middle & Top Grade MCB, Pedestal & Shell of Low Voltage Electrical ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd.
| Available Properties |
- Density
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Charpy Impact, Notched
- Volume Resistivity
- Comparative Tracking Index
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Processing Temperature
- Mold Temperature
- Dry Time
- Injection Pressure
|
|
|
|