KAIFA® M109-G20N MPPO Resin
Subcategory: Polyphenylene Ether/PPO; Thermoplastic; Polymer
Material Notes: 20% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group)
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Charpy Impact, Notched
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Mold Temperature
- Injection Pressure
- Cycle Time - Injection
- Screw Speed
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|