Alcoa KAMA 4100 Prime APET
Subcategory: Polyester, TP; Polyethylene Terephthalate (PET); Thermoplastic
Key Words: FDA Compliant: CFR 21 #177.1630
Material Notes: Capabilities- Gauge: .007” to .050” (178 to 1270µm)
- Width: 12” to 48” (305 to 1219mm)
- Core size: 6” standard, 3” and 8” available
- Roll O.D.: 29” standard, available up to 40”
- Available in clear, colored and tinted
- Graphic arts available
- Silicone coating available
- Medical grade material available
- 4 strategic manufacturing locations
Properties - Exceptional clarity and impact performance
- Good formability with great definition
- Faster forming cycles than PVC
- Excellent strength for tough POP applications
- 100% recyclable
- FDA accepted material
- Kosher material
- FDA compliant to CFR 21 #177.1630
Information provided by Alcoa Kama Co.
| Available Properties |
- Specific Gravity
- Viscosity Measurement
- Thickness
- Linear Mold Shrinkage
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Haze
- Transmission, Visible
- Processing Temperature
- Clarity, %
- Resistance to Alcohols
- Resistance to Alkalies
- Resistance to Fat, Grease, and Oil
- Resistance to Hydrocarbon Solvents
- Resistance to Strong Oxidozers
- Rsistance to Acid
- Yield, in²/lb/mil
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|