Alcoa KAMA 4223 Impact Modified RPET
Subcategory: Polyester, TP; Polyethylene Terephthalate (PET); Thermoplastic
Material Notes: Capabilities- Gauge: .009” to .045” (229 to 1143 µm)
- Width: 12” to 48” (305 to 1219mm)
- Core size: 6” standard, 3” and 8” available
- Roll O.D.: 29” standard, available up to 50”
- Silicone coating
- Clear, custom translucent and opaque colors
- Gloss and matte material available
- 3 strategic manufacturing locations
Properties - For demanding application requiring good impact resistance
- Impact modified for superior strength
- Ideal for deep draw, heavier gauge applications
- Exceptional clarity
Information provided by Alcoa Kama Co.
| Available Properties |
- Specific Gravity
- Viscosity Measurement
- Thickness
- Linear Mold Shrinkage
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Processing Temperature
- Resistance to Alcohols
- Resistance to Alkalies
- Resistance to Fat, Grease, and Oil
- Resistance to Hydrocarbon Solvents
- Resistance to Strong Oxidozers
- Rsistance to Acid
- Yield, in²/lb/mil
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|