Alcoa KAMA 4300 Petwich-PET
Subcategory: Polyester, TP; Polyethylene Terephthalate (PET); Thermoplastic
Material Notes: Capabilities- Gauge: .009” to .045” (229 to 1143 µm)
- Width: 12” to 48” (305 to 1219mm)
- Core size: 6” standard, 3” and 8” available
- Roll O.D.: 29” standard, available up to 40”
- Recycled content
- Silicone coating available
- Clear, custom translucent and opaque colors
- 4 strategic manufacturing locations
Properties - FDA acceptance for certain applications
- Recycled content
- Good clarity
- Excellent surface quality
- Improved economics for food content packing
- For environmentally responsible packaging
- 100% recyclable
- Kosher material
Information provided by Alcoa Kama Co.
| Available Properties |
- Specific Gravity
- Viscosity Measurement
- Thickness
- Linear Mold Shrinkage
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Haze
- Transmission, Visible
- Processing Temperature
- Clarity, %
- Resistance to Alcohols
- Resistance to Alkalies
- Resistance to Fat, Grease, and Oil
- Resistance to Hydrocarbon Solvents
- Resistance to Strong Oxidozers
- Rsistance to Acid
- Yield, in²/lb/mil
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|