Alcoa KAMA 6100 HDPE
Subcategory: Polyethylene; Thermoplastic; HDPE
Key Words: FDA Compliant: CFR 21 #177.1520
Material Notes: Capabilities- Gauge: .007” to .060” (178 to 1524µm)
- Width: 3” to 60” (76 to 1524mm)
- Core size: 6” standard, also available in 3” and 12”
- Roll O.D.: 29” standard, available up to 40”
- Silicone coating available
- Custom colors available
- Gloss and matte material
- Fragility material available
- Utility grade available
- Agricultural grades available
- Graphic arts grade available
Properties - Excellent moisture barrier properties
- Great for bulk food and consumer applications
- Ideal for protective, fragility packaging
- Great environmental stability for outdoor applications
- Excellent for low temperature applications
- FDA compliant to CFR 21#177.1520
Information provided by Alcoa Kama Co.
| Available Properties |
- Specific Gravity
- Thickness
- Linear Mold Shrinkage
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Processing Temperature
- Resistance to Alcohols
- Resistance to Alkalies
- Resistance to Fat, Grease, and Oil
- Resistance to Hydrocarbon Solvents
- Resistance to Strong Oxidozers
- Rsistance to Acid
- Yield, in²/lb/mil
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|