Keysor-Century KYNS PVC Copolymer Resin

 

Subcategory: Vinyl; Thermoplastic

Close Analogs:

Keysor-Century Corporation is no longer in business.

Material Notes:
A solution grade, high molecular weight vinyl chloride-vinyl acetate copolymer resin. 10% Vinyl acetate. KYNS is soluble in strong ketone systems to produce low solution rheological properties, and is highly resistant to moisture, wear, and chemicals. White Free Flowing Powder

Recommended for printing ink, top coat applications to vinyl film and sheeting, architectural finishes for masonry, wood, and steel, and for coatings that require high resistance to moisture, wear, or chemicals.

Particle size: Nil retained on 32 mesh. 40% max through 200 mesh. Max volatiles 1%

Property values are typical values. Information provided by Keysor-Century Corporation.

Available Properties
  • Density
  • Apparent Bulk Density
  • Brookfield Viscosity
  • Viscosity Measurement
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。