Keysor-Century KYNS PVC Copolymer Resin
Subcategory: Vinyl; Thermoplastic
Close Analogs: Keysor-Century Corporation is no longer in business.
Material Notes: A solution grade, high molecular weight vinyl chloride-vinyl acetate copolymer resin. 10% Vinyl acetate. KYNS is soluble in strong ketone systems to produce low solution rheological properties, and is highly resistant to moisture, wear, and chemicals. White Free Flowing Powder Recommended for printing ink, top coat applications to vinyl film and sheeting, architectural finishes for masonry, wood, and steel, and for coatings that require high resistance to moisture, wear, or chemicals. Particle size: Nil retained on 32 mesh. 40% max through 200 mesh. Max volatiles 1% Property values are typical values. Information provided by Keysor-Century Corporation.
| Available Properties |
- Density
- Apparent Bulk Density
- Brookfield Viscosity
- Viscosity Measurement
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|