Keysor-Century KC1201 Rigid PVC Extrusion Blow Molding Compound
Subcategory: Vinyl; Thermoplastic
Close Analogs: Keysor-Century Corporation is no longer in business.
Material Notes: A general purpose extrusion blow molding compound with an excellent balance of properties, offering outstanding clarity and gloss, high impact strength, and good color retention. KC1201's excellent dynamic thermal stability enables easy processability with a wide variety of equipment and conditions. This permits extended production runs with minimum maintenance and downtime, and maximum regrind recycling. It is available in glass clear, with various levels of blue tint, and in opaque white as free flowing pellets. Recommended for use in a wide variety of packages for non-food applications. Suitable for simple Boston Round design or complex shapes and sizes for cosmetics, cleaning fluids, floor waxes, shampoos, detergents, bleaches, and engine oil. Property values are typical values. Information provided by Keysor-Century Corporation.
| Available Properties |
- Density
- Hardness, Shore D
- Tensile Strength, Yield
- Modulus of Elasticity
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|