Keysor-Century KC1252 Rigid PVC Extrusion Blow Molding Compound
Subcategory: Vinyl; Thermoplastic
Close Analogs: Keysor-Century Corporation is no longer in business.
Material Notes: A food grade extrusion blow molding compound with an excellent combination of properties for high gloss and clarity, high impact strength, low gel, and low odor. KC1252 is formulated with an FDA-approved tin stabilizer to meet the 21CFR 178.2650 food additive regulation, and is produced under stringent manufacturing conditions limiting RVCM to minimum allowable levels. Its excellent dynamic thermal stability enables easy processability with a wide variety of equipment and conditions. This permits extended production runs with minimum maintenance and downtime, and maximum regrind recycling. It is available in clear, with various levels of blue tint as free flowing pellets. Recommended for product packages requiring compliance with FDA additive regulations to containerize liquor, edible oils, mouthwash, dry foods, and cosmetics. Property values are typical values. Information provided by Keysor-Century Corporation.
| Available Properties |
- Density
- Hardness, Shore D
- Tensile Strength, Yield
- Modulus of Elasticity
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|