Keysor-Century B460C Clear Vinyl Record Compound
Subcategory: Vinyl; Thermoplastic
Close Analogs: Keysor-Century Corporation is no longer in business.
Material Notes: A rigid vinyl chloride-vinyl acetate copolymer compression molding compound. Keysor B460C is a transparent compound that is virtually clear, made with a slight blue tint free flowing pellets. Plastograph 800 M-g per KC 08. T.O. is 100 sec per ASTM D-1238. 0.5% Volatiles. Recommended for standard phonograph record manufacturing and specialized molding applications. Property values are typical values. Information provided by Keysor-Century Corporation.
| Available Properties |
- Density
- Apparent Bulk Density
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|