KiON CERASET® POLYSILOXAZANE 12 Ambient-Cure Ceramic Precursor
Subcategory: Thermoset; Polymer
Material Notes: General DescriptionKiON Ceraset Polysiloxazane 12 is a clear, low viscosity liquid polysilazane that can be used by itself or in combination with ceramic or metal particulate for a variety of thin cross-section ceramic applications, such as sealant coatings or in ceramic membranes or filters. KiON Ceraset Polysiloxazane 12 is designed to cure at ambient temperature through a moisture-induced crosslinking mechanism. When applied to a substrate, KiON Ceraset Polysiloxazane 12 will be dry to the touch within 1 hour (depending on the relative humidity), and thoroughly dry over the course of several hours. KiON Ceraset Polysiloxazane 12 has a slower cure profile than KiON Ceraset Polysiloxazane 33. Pyrolysis results in the formation of an amorphous, non-glassy silicon oxycarbonitride ceramic. Applications Sealant for Porous Ceramics, SiC / Si3N4 Coatings for C/C Composites, Spin Coating, and Ceramic MEMS. Information provided by KiON Corporation
| Available Properties |
- Density
- Viscosity
- Refractive Index
- %Resin
- Appearance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|