KiON HTA 1500 SLOW CURE Ambient-Curable, High Temperature Coating Resin

 

Subcategory: Thermoset; Polymer

Material Notes:
General Description

KiON HTA 1500 Slow Cure is a clear, colorless, low viscosity liquid polysiloxazane coating resin that is specially designed for use in the formulation of ambient-curable coatings capable of withstanding operating temperatures of 1500 ºF or above. KiON HTA 1500 Slow Cure is supplied as a 100% “solids” liquid of low viscosity. After application, a coating prepared using KiON HTA 1500 Slow Cure will be dry-to-touch within 1 hour, and will be ready-for-use after 1 day. KiON HTA 1500 Slow Cure can be blended with a variety of pigments, such as metal powders (zinc, aluminum, stainless steel), ceramic powders (silicon carbide, aluminum oxide, silicon nitride), or the like. Such compositions can be formulated with or without solvent and can be applied by dipping, spraying, or brushing onto a variety of substrates – metal, glass, ceramic, polymeric. For ultra-high temperature formulations, the coated part is then heated to at least 850 ºF to promote conversion of the polymer to ceramic. Depending on the exact formulation, coating operating temperatures of 1500 ºF or above can be achieved.

Applications

High Temperature Coatings and Thermally Stable Corrosion Coatings

Information provided by KiON Corporation

Available Properties
  • Density
  • Viscosity
  • Flash Point
  • Refractive Index
  • %Resin
  • Appearance
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。