KiON URETHANE HYBRID CLEAR COAT Pack B Heat-Curable Polysilazane-Based Hybrid Spray Coat
Subcategory: Thermoset; Polymer
Material Notes: General DescriptionKiON Urethane Hybrid Clear Coat is a ready-to-use clear coat containing both polysilazane and polyurethane components that can be thermally-cured to provide an oxidation and corrosion-resistant clear or pigmented finish. KiON Urethane Hybrid Clear Coat is furnished as a 2-Pack system that can be applied by spray, dip, and brush coating techniques. It cures upon heating to temperatures of between 293 °F and 311 °F for 1 hour. KiON Urethane Hybrid Clear Coat provides a clear, protective coating for both ferrous and non-ferrous metals and alloys, ceramics, glass, etc. In addition, KiON Urethane Hybrid Clear Coat has excellent “weatherability”, UV resistance, hardness and abrasion resistance. Applications Clear, protective coatings for both ferrous and non-ferrous metals and alloys, clear automotive finishes, thermally durable coatings, and industrial, infrastructure and marine coatings. Information provided by KiON Corporation
| Available Properties |
- Density
- Volatile Organic Compounds (VOC) Content
- Viscosity
- Flash Point
- Gloss
- %Resin
- Appearance
- Pencil Hardness ASTM D 3363
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|