KiON EH66 EPOXY HARDENER Polysilazane-Based Epoxy Hardner
Subcategory: Thermoset; Polymer
Material Notes: General DescriptionKiON EH66 Epoxy Hardener is a specially designed product in which a KiON polysilazane is reacted with a conventional amine hardener for epoxy resins. KiON EH66 Epoxy Hardener enables the formulation of ambient temperature curing, 2K epoxies having enhanced adhesion and UV stability. Applications Epoxy “hybrid” coatings and adhesives for a wide variety of substrates and materials. KiON epoxy “hybrid” polymers prepared using KiON EH66 Epoxy Hardener adhere tenaciously to a wide range of materials including metals, polymers, graphite, and glass. Information provided by KiON Corporation
| Available Properties |
- Density
- Viscosity
- Flash Point
- Gel Time
- %Resin
- Appearance
- Weight per Active H
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|