KKPC KOSYN SOL 5520 Solution Styrene Butadiene Rubber (S-SBR)
Subcategory: Styrene-Butadiene; Elastomer, TS; Thermoset
Material Notes: Solution Styrene Butadiene Rubber (S-SBR) Characteristics: This product is made by solution polymerization under which styrene and butadiene react in organic solvent using alkyl-lithium catalyst. It is superior to SBR, which is made by emulsion polymerization, in processability, visco-elasticity and low temperature properties. Also, the products' properties can be adjusted to the purpose of consumption according to the proper proportion of styrene content, the micro structure and the molecular weight. Applications: Shoes, Soles, Tires, Machine Parts, Energy-saving Tires, High-efficiency Tires Additional Notes: Bound Styrene: 23.7% cis-1,4 Contents: 25% trans-1,4 Contents: 39% Vinyl Contents: 39% Dynamic Test: GABO Qualimeter (11Hz) (TAN) 0°C: 0.326 10°C: 0.214 60°C: 0.125 70°C: 0.116 This product is so sensitive to sunlight and humidity that it can be tarnished and caused deterioration of quality if exposed. It is recommended to store it in cool and shady area lest it should be exposed to direct sunlight. Do not expose to incompatible materials or contaminants. Data provided by Korea Kumho Petrochemical Co., Ltd.
| Available Properties |
- Mooney Viscosity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- 300% Modulus
- Glass Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|