KKPC KOSYN KBR 31 Polybutadiene Rubber (High cis BR)
Subcategory: Elastomer, TS; Thermoset
Material Notes: Polybutadiene Rubber (High cis BR) Characteristics: KBR 31 contains an aromatic oil additive. Polybutadiene Rubber (BR), which has three kinds of bond structure of cis-1,4, trans-1,4, vinyl, is simple polymer made from 1,3-butadiene by solution polymerization, and it is classified to High cis BR and Low cis BR according to the cis-1,4 content. High cis BR containing over 94% cis-1,4 is superior in abrasion resistance, elasticity, age resistance and water resistance. As the secondary transition temperature is about -100? low, it is most widely utilized together with SBR. Applications: Conveyor belting, tires (superior for snow tire tread). Additional Notes: Extender Oil: 37.5; Aromatic Stabilizer: Non-Polluting cis-1,4 Contents: 95% Volatile Matter: 0.3% Ash Content: 0.1% This product is so sensitive to sunlight and humidity that it can be tarnished and caused deterioration of quality if exposed. It is recommended to store it in cool and shady area lest it should be exposed to direct sunlight. Do not expose to incompatible materials or contaminants. Data provided by Korea Kumho Petrochemical Co., Ltd.
| Available Properties |
- Density
- Mooney Viscosity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- 300% Modulus
- Rebound
- Flex Crack Resistance
- Tear Strength
- Abrasion
- Compression Set
- Compression Set, Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|