KKPC Kumho RM 21 High Styrene Resin Materbatch (HSR)

 

Subcategory: Styrene-Butadiene; Elastomer, TS; Thermoset

Material Notes:
High Styrene Resin Materbatch (HSR)

Characteristics: KOSYN KHS is produced by mixing SBR 1502 of 23.5% styrene and high styrene resin latex at high temperature. It works as plasticizer which improves processability in rubber compounding, and has superior abrasion resistance, tear resistance and flex crack resistance. Also, it can hold up good physical properties with fillers. This product has superior compounding dispersibility and processability in addition to promoting the stiffness of manufactured goods.

Applications: Industrial products such as shoe parts with high-stiffness, sponges, cars, tires

Additional Notes:
Bound Styrene: 21%
Stabilizer: Non-Staining
Appearance: Bale
Cured Rubber: Press cured 50 minutes at 145°C

This product is so sensitive to sunlight and humidity that it can be tarnished and caused deterioration of quality if exposed. It is recommended to store it in cool and shady area lest it should be exposed to direct sunlight. Do not expose to incompatible materials or contaminants.

Data provided by Korea Kumho Petrochemical Co., Ltd.

Available Properties
  • Density
  • Mooney Viscosity
  • Hardness, Shore A
  • Tensile Strength, Ultimate
  • Elongation at Break
  • 300% Modulus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。