KKPC KOSYN KTR 602 Thermoplastic Elastomer (TPE)
Subcategory: Elastomer, TPE; Thermoplastic; Styrenic TPE
Material Notes: Thermoplastic Elastomer (TPE) Characteristics: KOSYN KTR101 is linear block copolymer made by solution polymerization which polymerizes butadiene and styrene in organic solvent. It is thermoplastics free of vulcanization and has superior tensile strength and elasticity. Applications: Asphalt roofing, waterproof agent, modifier and adhesives. Additional Notes: Bound Styrene: 40% Volatile Matter: 0.5%; ASTM D1416 Ash Content: 0.3%; ASTM D1416 This product is so sensitive to sunlight and humidity that it can be tarnished and caused deterioration of quality if exposed. It is recommended to store it in cool and shady area lest it should be exposed to direct sunlight. Do not expose to incompatible materials or contaminants. Data provided by Korea Kumho Petrochemical Co., Ltd.
| Available Properties |
- Density
- Brookfield Viscosity
- Melt Flow
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|