KKPC KOSYN KSL 106 Styrene-Butadiene Latex
Subcategory: Styrene-Butadiene; Adhesive; Elastomer, TS; Thermoset
Material Notes: Styrene-Butadiene Latex Characteristics: KOSYN KSL 100 series are carboxy metamorphic styrene-butadiene latexes. They have a soft touch and high adhesive force. Applications: Carpet Backing, Adhesive for textile goods, adhesion of sandpaper, binder for Non-woven Fabric This product is so sensitive to sunlight and humidity that it can be tarnished and caused deterioration of quality if exposed. It is recommended to store it in cool and shady area lest it should be exposed to direct sunlight. Do not expose to incompatible materials or contaminants. Data provided by Korea Kumho Petrochemical Co., Ltd.
| Available Properties |
- Solids Content
- pH
- Viscosity
|
|
|
|