Kydex® 100 Acrylic/PVC Thermoplastic Sheet
Subcategory: Vinyl; Acrylic; Thermoplastic
Key Words: Polyvinylchloride; PMMA; Polymethylmethacrylate
Material Notes: High impact fire rated sheet Applications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones. Hidden parts for equipment such as vending machines, air ducts, grills. Orthopedic braces, medical equipment parts, in-store displays, electrical equipment Features: Superior formability for deep or hard to form parts or where good finished detail is required. Kydex 100 is more rigid than most other thermoplastics resulting in parts that will deform less when loaded. Offers unsurpassed resistance to breakage. Meets the highest standard for chemical resistance for thermoplastic materials. Recognized by Underwriter's Laboratories Inc. for Standard 94 V-0 and 5V and UL 746C in all gauges and colors. Passes Motor Vehicle Safety Standards (MVSS 302). Radiant Panel: 22.5 as per ASTM E162 Fabrication: Excellent forming properties result in uniform wall thicknesses and crisp detail, plus easy machining and fabricating using conventional methods, further expanding finished part possibilities. Data provided by the Kleerdex Company.
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Hardness, Rockwell R
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength @ Yield
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Ultimate Bearing Strength
- Shear Strength
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Tensile Impact Strength
- Taber Abrasion, mg/1000 Cycles
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Arc Resistance
- Comparative Tracking Index
- Hot Wire Ignition, HWI
- High Amp Arc Ignition, HAI
- High Voltage Arc-Tracking Rate, HVTR
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Deflection Temperature at 1.8 MPa (264 psi)
- UL RTI, Electrical
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
- Oxygen Index
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|