Kydex® 100 AS Acrylic/PVC Thermoplastic Sheet
Subcategory: Vinyl; Acrylic; Thermoplastic
Key Words: Polyvinylchloride; PMMA; Polymethylmethacrylate
Material Notes: Anti-static sheet Applications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones, internal parts for electrical and electronic equipment, medical equipment parts, carrying trays, carts, and trolleys for sensitive electrical components. Features: Unlike other anti-static thermoplastic sheets, Kydex 100AS retains its anti-static properties even after thermoforming. Also it is available in a multitude of colors. For deep or hard to for parts or where good finished detail is required, Kydex 100AS is unsurpassed. It meets the highest standard for chemical resistance for thermoplastic materials. Fabrication: Excellent forming properties result in uniform wall thicknesses and crisp detail, plus easy machining and fabricating using conventional methods, further expanding finished part possibilities. Data provided by the Kleerdex Company.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Flexural Yield Strength
- Izod Impact, Notched
- Surface Resistivity per Square
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|