Kydex® 115 Acrylic/PVC Thermoplastic Sheet

 

Subcategory: Vinyl; Acrylic; Thermoplastic

Key Words: Polyvinylchloride; PMMA; Polymethylmethacrylate

Material Notes:
High rigidity sheet for ceiling panels

Applications: Ceiling panels in clean rooms, computer rooms, laboratories, food, dairy, and pharmaceutical plants, and other environments where a high degree of cleanliness is required, decorative panels, sound diffusers

Features: Kydex 115 meets the criteria for flame spread and smoke development that determines Class I/A compliance using ASTM E84 methodology. It is ideal for applications such as ceiling panels where the product must be routinely removed and/or cleaned for maintenance. It provides superior impact protection and well not chip, crack, or flake. Color is integral throughout each sheet. Kydex 115 has excellent chemical resistance allowing for the removal of tougher stains with stronger cleaning agents without damaging the surface of the sheet. This high rigidity fire rated sheet is a non-porous, tough, chemical resistant material. Clean Room Class 10 Federal Standard 209D.

Fabrication: Excellent forming properties result in uniform wall thicknesses and crisp detail, plus easy machining and fabricating using conventional methods, further expanding finished part possibilities.

Data provided by the Kleerdex Company.

Available Properties
  • Density
  • Water Absorption
  • Water Absorption at Saturation
  • Hardness, Rockwell R
  • Tensile Strength, Ultimate
  • Modulus of Elasticity
  • Flexural Yield Strength
  • Izod Impact, Notched
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Flammability Test
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。