Kydex® 115 Acrylic/PVC Thermoplastic Sheet
Subcategory: Vinyl; Acrylic; Thermoplastic
Key Words: Polyvinylchloride; PMMA; Polymethylmethacrylate
Material Notes: High rigidity sheet for ceiling panels Applications: Ceiling panels in clean rooms, computer rooms, laboratories, food, dairy, and pharmaceutical plants, and other environments where a high degree of cleanliness is required, decorative panels, sound diffusers Features: Kydex 115 meets the criteria for flame spread and smoke development that determines Class I/A compliance using ASTM E84 methodology. It is ideal for applications such as ceiling panels where the product must be routinely removed and/or cleaned for maintenance. It provides superior impact protection and well not chip, crack, or flake. Color is integral throughout each sheet. Kydex 115 has excellent chemical resistance allowing for the removal of tougher stains with stronger cleaning agents without damaging the surface of the sheet. This high rigidity fire rated sheet is a non-porous, tough, chemical resistant material. Clean Room Class 10 Federal Standard 209D. Fabrication: Excellent forming properties result in uniform wall thicknesses and crisp detail, plus easy machining and fabricating using conventional methods, further expanding finished part possibilities. Data provided by the Kleerdex Company.
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Flexural Yield Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability Test
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|