Kydex® 160 Acrylic/PVC Thermoplastic Sheet
Subcategory: Vinyl; Acrylic; Thermoplastic
Key Words: Polyvinylchloride; PMMA; Polymethylmethacrylate
Material Notes: Class I/A rated thermoplastic sheet Applications: Interior ductwork and chutes, laboratory hoods, shower/tub shrouds, acoustical applications, decorative ceilings, abuse resistant surfacing for counters, exhibits, partitions, doors Features: Kydex 160 sheet is more resistant to a wider range of concentrated chemicals than any other thermoplastic. Its superior chemical resistance allows for excellent cleanability because stronger clearing agents can be sued with no discoloration or surface damage to the material. Fabrication: Kydex 160 has good formability and extensibility a and is extremely easy to work with once formed. Data provided by the Kleerdex Company.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Flexural Yield Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|