Kydex® 550 Acrylic/PVC Thermoplastic Sheet

 

Subcategory: Vinyl; Acrylic; Thermoplastic

Key Words: Polyvinylchloride; PMMA; Polymethylmethacrylate

Material Notes:
Weatherable monolithic sheet

Applications: Housings for equipment, recreational vehicles and truck parts, safety equipment, building products, signage

Features: Kydex 550 offers the properties of "Kydex" in a weatherable formulation. It is highly impact resistant as measured by the notched Izod impact resistance test. It is fire retardant with a UL 94 V-0 rating as measured by an independent testing laboratory. It eliminates the problems often associated with capped sheet products.

Fabrication: Excellent forming properties result in uniform wall thicknesses and crisp detail, plus easy machining and fabricating using conventional methods, further expanding finished part possibilities.

Data provided by the Kleerdex Company.

Available Properties
  • Density
  • Linear Mold Shrinkage
  • Hardness, Rockwell R
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Modulus of Elasticity
  • Flexural Yield Strength
  • Izod Impact, Notched
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Flammability, UL94
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。