Kydex® 6185 Thermoplastic Sheet
Subcategory: Thermoplastic
Material Notes: High temperature aircraft grade Applications: Aircraft interior components examples include: air ducts, window reveals, instrument panels, toilet shrouds, armrests Features: Kydex 6185 is a proprietary thermoplastic sheet with improved heat distortion temperature (HDT) for higher in-service temperatures while providing excellent extensibility, good impact resistance, and excellent solvent resistance. It meets FAR 25.853(a) for use in aircraft interior parts. Maximum recommended service temperature is approx. 82-90°C depending on thermoforming technique and application. Kydex 6185 sheet is designed primarily for use in small aircraft interiors particularly the interior of helicopters which often experience temperature in excess of 82°C, but also is appropriate for other applications where high in-service temperatures may occur. Fabrication: Excellent forming properties result in uniform wall thicknesses and crisp detail, plus easy machining and fabricating using conventional methods, further expanding finished part possibilities. Data provided by the Kleerdex Company.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Flexural Yield Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|