Kydex® CL2 PVC Sheet
Subcategory: Vinyl; Thermoplastic
Key Words: Polyvinylchloride
Material Notes: Clear high impact rigid PVC sheet Applications: Semiconductor processing equipment, etching and plating tanks, machined and fabricated parts, scrubbers, hoods, ducts, and other protective equipment, thermoformed parts, aircraft interior components Features: Kydex CL2 has excellent chemical and corrosion resistance. Kydex CL2 is flame retardant and meets UL 94 HOB requirements. It has a showcase quality surface. It is stress relieved, square, flat sheet. It stays functional and attractive over time in a wide range of demanding applications. Kydex CL2 has a higher impact resistance than other clear PVC or acrylic sheet grades. Fabrication: Kydex CL2 is thermoformable and is easily fabricated, welded, a and machined for further expanding finished part possibilities. Data provided by the Kleerdex Company.
| Available Properties |
- Density
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Haze
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|