Kydex® T Acrylic/PVC Thermoplastic Sheet
Subcategory: Vinyl; Acrylic; Thermoplastic
Key Words: Polyvinylchloride; PMMA; Polymethylmethacrylate
Material Notes: Impact resistant fire rated sheet Applications: External housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones, internal parts for equipment such as vending machines, air ducts, grilles, orthopedic braces, medical equipment parts, in-store displays, electrical equipment and any components requiring an UL 94 V-0 rating. Features: Kydex T is formulated to substitute for FR ABS sheet with competitive pricing but superior cost and performance. It has higher breakage resistance as measured by the Notched Izod test than competitive thermoplastics. Kydex T is available in eight gauges, in nine textures, a large variety of colors, custom blank sizes, and very low minimums. Kydex T is among the most rigid of thermoforming materials. Fabrication: Kydex T is easy to form with excellent part definition and deep-draw characteristics. It forms with similar forming times to FR-ABS making it easy transition from competitive products. Data provided by the Kleerdex Company.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Flexural Yield Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- UL RTI, Electrical
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|