Vinyloy™ 100 Acrylic/PVC Thermoplastic Sheet
Subcategory: Vinyl; Acrylic; Thermoplastic
Key Words: Polyvinylchloride; PMMA; Polymethylmethacrylate
Material Notes: Utility grade Applications: Vinyloy 100 sheet is a fire retardant that can be used to substitute effectively for ABS and other utility grade thermoplastics. Features: Vinyloy 100 sheet is a recycled grade of proprietary acrylic/PVC thermoplastic sheet that is cost competitive with other utility grades of thermoplastic sheet while offering improved performance. Vinyloy 100 sheet is UL recognized 94 V-0 and 5V. Fabrication: Excellent forming properties result in uniform wall thicknesses and crisp detail, plus easy machining and fabricating using conventional methods, further expanding finished part possibilities. Data provided by the Kleerdex Company.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Flexural Yield Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|