KOSTAT BK-STAT P048BK PP Compound
Subcategory: Polypropylene; Thermoplastic
Material Notes: BK-STAT Compounds are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanliness requirements in comparison to other materials based on Hygroscopic Antistats, Inherently Conductive Polymer Coating, or Conductive Fillers such as carbon fibers and carbon blacks.BK-STAT Compounds exhibit superior property and processing characteristics compared with other competitive IDP based compounds. Special Features: - Superior Permanent Static Dissipation
- Excellent Wear Resistance
- Humidity Insensitivity
- Exceptionally High Impact Resistance
- No Particle Generation
- Excellent Processibility
Applications: - Semiconductor Packaging
- LCD Packaging
- Electrical & Electronics
- Medical Devices
- Storage Disks
- Appliances
- Consumer Goods
- Clean Room Accessories
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Tensile Strength, Yield
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Surface Resistivity per Square
- Static Decay
- Deflection Temperature at 1.8 MPa (264 psi)
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|