KOSTAT 7440 Conductive ABS Compound
Subcategory: ABS Polymer; Thermoplastic
Material Notes: KOSTAT 7440 is a conductive thermoplastic compound based on Acrylonitrile Butadiene Styrene and a special carbon black. KOSTAT 7440 is not dependant on atmospheric conditions and is used for ESD injection molded products.Special Features This product exhibits high conductivity, easy processing, smooth sheet surface, and tight dimensional tolerances after injection molding. This makes KOSTAT 7440 suitable for various injection molding applications. Applications: KOSTAT 7440 is recommended for electronics packaging such as ESD Trays and other injection molded products.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistivity per Square
- Deflection Temperature at 1.8 MPa (264 psi)
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|