Kraton® D2104 "Ready to use" Compound
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes: Normal procedures for handling dust producing solids should be followed when handling and storing KRATON Polymer pellets. Compounding KRATON Polymers in high shear equipment can cause a significant rise in temperature. Do not exceed 225-230°C (437-446°F) for KRATON D polymers and compounds and 280-285°C (536-545°F) for KRATON G Polymers and compounds. Maintain a fire watch if these temperatures are reached. KRATON Polymer products (the neat resin or the base product) are high molecular weight polymers which by all accounts are non-toxic and biologically inactive. KRATON Polymers and compounds can accumulate electrostatic charges when rubbed, chafed or abraded and processing equipment should have a way of dissipating these charges. Applications: Injection molded or extruded items, sporting goods, film. Information provided by the manufacturer, Kraton® Polymers.
| Available Properties |
- Specific Gravity
- Melt Flow
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Tear Strength
- Electrical Resistivity
- Dielectric Strength
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|